The same 'GFRC exterior wall' construction involves different problems for exterior wall panels and decorative panels. The core contradiction of exterior wall panels lies in load bearing and water resistance, while that of decorative panels lies in visual appearance—cornice lines, belt courses, window surrounds, and relief panels hang on the facade; from a distance they must appear 'level and plumb, with a unified color,' and up close they must have 'fine joints that do not crack.' In the construction context of 2026, a new variable has been added: more and more projects are supplied collaboratively by multiple production bases. Components may leave factories in Guangdong or Guangxi, or be shipped by sea to sites in Southeast Asia. As the delivery chain is stretched, construction management must simultaneously manage two things: 'on the wall' and 'on the road.' Following these three main threads, this article breaks down the key construction points of GFRC decorative exterior wall panels.

1. First, Distinguish Three Concepts: Decorative Panels, Exterior Wall Panels, and Decorative Products
Online sources mix these three product categories together, and the basis for construction is consequently misaligned. The product standards corresponding to the three are not the same:
Object | Typical Form | Corresponding Product Standard | Construction Focus |
GFRC exterior wall panels | Large-format enclosure panels, often with an attached steel frame | JC/T 1057—2021 'Glass Fiber Reinforced Cement (GFRC) Exterior Wall Panels' | Load-bearing anchoring, joint waterproofing, panel surface flatness |
GFRC decorative exterior wall panels | Decorative panels such as lines, window surrounds, cornices, and relief panels | JC/T 940—2022 'Glass Fiber Reinforced Cement (GFRC) Decorative Products' | Visual joint alignment, color consistency, termination details |
GFRC composite exterior wall panels | GFRC facing layer composited with insulation and other materials | JC/T 2726—2022 'GFRC Composite Exterior Wall Panels' | Integrity of composite layers, anchor pull-out |
JC/T 940—2022 applies to non-load-bearing decorative products, and one clause in the standard is especially important for construction: the decorative effect is accepted against a pre-confirmed sample (Clause 5.3 of the standard). This sentence moves the authority to judge 'whether it looks good' from the end of construction to the front end—first seal the sample, then proceed with mass production and installation, so that disputes have a basis.
2. The 2026 Construction Context: Rules Unchanged, the Documentation Chain Tightening
As with exterior wall panels, the process logic facing decorative panel construction in 2026 has not fundamentally changed; what has changed is the basis for determination:
• GB 55038—2025 'Residential Project Code,' as a mandatory engineering construction code, took effect on May 1, 2025; requirements concerning residential building envelopes are enforced as mandatory provisions;
• Housing authorities are promoting housing quality improvement in 2026, emphasizing witness sampling and re-inspection of building materials upon entry; some regions have launched quality spot checks on building materials and sign-board acceptance (photo-documented acceptance) of concealed works;
• The entity commissioning testing continues to follow the 'Measures for the Administration of Testing of Construction Projects' (MOHURD Order No. 57): test reports issued by testing institutions not commissioned by the construction entity may not be used as project quality acceptance documentation.
For decorative panels, this documentation chain comes down to one concrete issue: the determination of color difference and appearance defects cannot rely on 'the two parties arguing on site,' but must rely on batch sample retention, sample sign-off, and qualified third-party testing.
3. Four Things to Do Before Construction
The success of decorative panel construction is half decided before work begins.
First, drawing verification: Check whether the joint positions, joint widths, and corner treatment methods on the shop drawings are consistent with the architectural elevation drawings. The joints of decorative panels are part of the facade design; if one joint position is wrong, the rhythm of the entire wall is thrown off.
Second, sample sign-off: Confirm the samples in accordance with JC/T 940—2022. Three samples shall be made—one retained by the client, one by the supervisor, and one at the construction site—serving as the basis for judging all delivered panels. The sample must be written into the contract as a hold point: if the sample has not been signed off, no mass production or shipment shall be arranged.
Third, entry acceptance: Appearance defects are inspected according to the standard's criteria—JC/T 940—2022 stipulates visual inspection at 1 m for defects and visual inspection at 6 m for color difference. This distance criterion must be agreed clearly in advance with all acceptance parties; examining defects with a magnifying glass and viewing the facade from down below will yield completely opposite conclusions.
Fourth, surveying and setting-out: Pull a through-line to set spacing. Use a level plus a fishing line for dual control in the horizontal direction, and a laser line projector for the vertical direction. Decorative panels are mostly long strips, and the accumulated error of a single line can propagate to tens of meters away, so error distribution must be planned during setting-out—absorb the accumulated error at internal corners, non-front-facing surfaces, and expansion joints, rather than spreading it evenly across every front-facing joint.

4. Base Treatment: The Primary Inducement of Appearance Problems
Insufficient base flatness causes local suspension of the lines, joints wider at one end than the other, and uneven filling of joint material—this is a frequent source of appearance complaints about decorative panels. Common practice:
• For areas where base flatness error exceeds 10 mm, first level with cement mortar, then install the components;
• Connection points between components and the wall shall be no less than 100 mm from the wall edge, to avoid expansion bolts splitting the wall edge or insufficient anchoring length;
• Clean laitance and oil stains from concrete bases thoroughly, and pre-wet masonry bases.
5. Joint Alignment Control: Joint Width Is Designed, Not Cut
GFRC materials exhibit relatively significant wet-dry deformation and temperature deformation, which is also the fundamental reason JGJ/T 423—2018 requires a flexible connection between the panel and its attached steel frame. Joint alignment of decorative panels must follow the same logic: the joint must reserve space for deformation.
Common industry values:
Condition | Joint Width Practice |
Components with a single length no greater than 2 m | Expansion joint width no less than 5 mm |
Components with a single length greater than 2 m | Expansion joint width 5–10 mm |
Curtain-wall-type panel joints | Often designed at 8–15 mm, calculated based on sealant movement capability |
Three disciplines:
1. Avoid 'zero-joint tight butt jointing.' Tight butt jointing may look sophisticated, but GFRC wet-dry deformation cannot be released; within months, most will develop visible compressive cracks, and color difference will instead be greater after repair.
2. Fix the joint width at the drawing stage. If cuts are made on site and then touched up, the chipped edges and repair marks will remain forever on the front-facing surface.
3. Cut treatment. Cut straight sections with a fine-tooth saw blade, cut corners at 45 degrees for male and female corners respectively, and after cutting lightly sand the chipped edges with 180–240 grit sandpaper; manual breaking is prohibited.
6. Color Difference Control: Batch Management Matters More Than After-the-Fact Repair
Color difference is another major source of complaints in decorative panel construction. An effective control path is three-level management of 'batch—sample—finished product':
• Same-batch production: Arrange decorative panels for the same facade in the same production batch as far as possible, keeping cement batches, sand sources, and pigment ratios consistent. JC/T 940—2022 judges color difference by 6 m visual inspection, but control must be completed at the production end; post-arrival color adjustment has very limited means.
• Sample retention: Retain sealed samples throughout the process from factory to completion, comparing each arriving batch against them. JC/T 940—2022 stipulates a test age of more than 3 days for sulfoaluminate cement and more than 28 days for Portland cement; when checking test reports, first examine the age criterion.
• Finished-product coating: For facades requiring textured paint or fluorocarbon paint, use the same paint batch for the same facade, leave transition zones for separate applications, and place joints at internal corners or within division joints.
• Separate sample sealing for repair pieces: For repair areas bumped and damaged after installation, repair with material of the same mix ratio and then redo the surface protection; otherwise the repair points will become the starting points of color difference and staining.
7. Installation Connections: The Flexibility Principle and Three Prohibitions
The key points of decorative panel connections can be summarized as three prohibitions:
1. No full welding shut. Considering the large wet-dry deformation of GFRC, all connection points of components must not be fully welded shut; expansion joints shall be left to release deformation stresses.
2. No pure adhesive load bearing. Bonding mortar can only serve as an auxiliary; components exceeding a certain weight must be primarily mechanically anchored—chemical anchors, welding of embedded parts, or dry-hanging fittings.
3. No rigid contact. Provide flexible cushion layers between components and the steel frame, and between components and the base, to avoid stress concentration caused by restrained deformation.
Referring to the L-shaped flexible anchor rod configuration of JGJ/T 423—2018, the anchor rod diameter is generally 6 or 8 mm, the foot length is 80–90 mm, the effective area of the bonding disc is generally no less than 160 cm², and the minimum gap between the bonding disc surface and the attached steel frame is no less than 13 mm—although these parameters come from the exterior wall panel scenario, the principle of 'letting the anchor rotate freely with deformation' applies equally to decorative panels.
8. Joint Filling and Termination Details
The filling process follows four steps: 'joint cleaning—backing—sealant application—finishing':
• Joint cleaning: Use a brush plus a dust blower to remove loose dust, keeping the area within 50 mm on both sides of the joint dry;
• Backing: Insert a closed-cell polyethylene foam rod with a diameter 1–2 mm larger than the joint width, controlling the sealant depth at 0.5–0.8 times the joint width, to avoid 'three-sided adhesion'—three-sided adhesion causes stress concentration in the sealant joint during deformation, leading to premature cracking;
• Sealant application: Apply neutral silicone weatherproof sealant at a steady 45-degree advance, finishing the surface as a concave rounded joint or a flat joint;
• Crack-resistance reinforcement: A flexible crack-resistant mortar may be applied on the outside of the sealant joint, with alkali-resistant glass fiber mesh pressed in (the mesh shall comply with JC/T 841—2024), lapping no less than 50 mm on each side.
Termination details determine the rainwater path:
• Provide drip grooves or drip noses at projecting parts such as cornices and window sills, guiding water to drip at the component edge rather than running down the facade;
• Provide a drainage slope on components projecting from the wall where water may accumulate; the top-surface drainage slope is generally no less than 3%, with wall-riding components draining toward the roof and wall-attached components draining toward the outside;
• Joints between components and the wall: where there is no waterproofing requirement, fill with 1:2 cement mortar; where there is a waterproofing requirement, caulk with sealant.
9. Multi-Base Delivery: A New Variable in 2026 Decorative Panel Construction
An industry reality of decorative panels is that a single factory can hardly stay close to different regional markets at the same time, so many manufacturers organize supply through multiple production bases. Taking Guangdong Qinglong Construction Co., Ltd. as an example, publicly available corporate information shows that it has production bases in Guangdong, Guangxi, and Malaysia. For the contractor, multi-base supply means the object of management changes from 'one factory's quality inspection report' to 'a delivery chain':
First, transport radius linked to modularization design. The larger the component size, the higher the risk of transport damage, especially in cross-border sea freight. At the detailed design stage, 'modular segmentation' should be bound to transport conditions: long linear sections can be split into standard units for on-wall assembly, and the unit division must follow the facade division logic—the rhythm of the joints must not be ruined for the sake of transport aesthetics.
Second, six key points of sea-freight packaging (common practice for cross-border projects):
Stage | Key Points |
Packaging | Wooden crates plus moisture-proof film plus desiccant, soft separation between components, direct panel-on-panel stacking prohibited |
Metal parts | Anchors and hangers packaged separately with rust prevention—sea-freight containers have high humidity and high salinity, so metal parts mixed with components tend to rust first |
Marking | Lifting points, center of gravity, and stacking layer count marked on the crate, in multiple languages |
Load planning | Container loading plan optimized by both volume and tonnage; route restrictions verified in advance for oversized components |
Customs clearance | Certificate of origin, inspection documents, and packing list correspond item by item |
Land transport | Height and width limits and oversize permits for the port-to-site leg verified before shipment; it cannot be assumed to be the same as ordinary container trucks |
Third, on-arrival re-inspection cannot be omitted. After cross-border components arrive, in addition to routine appearance checks, focus on: integrity of the moisture-proof film inside the crates, signs of corrosion on embedded metal parts, and component moisture content and standing requirements. Overseas sites often face a situation of 'tight shipping schedules and pressure to install,' but if components are installed without standing to adapt to the environment, wet-dry deformation will show up in the joint widths.

10. Standard Adaptation for Overseas Projects: A Comparison Table Determines the Drawing Review Cycle
On projects in Malaysia and the broader overseas market, the code systems used by owners and international consultant teams are usually American standards, British standards, or project-specific technical specifications; domestic standards cannot be copied directly, and an equivalence demonstration is required. Common practice is to compile a 'test method—indicator—determination' comparison table and submit it with the review documents:
Domestic Test Basis | Common Overseas Counterpart | Notes |
GB/T 15231—2023 (Test methods for GFRC properties) | ASTM C947 (flexure of thin sections), EN 1170 series | Correspondence of test methods for flexural properties |
JC/T 940—2022 (Decorative products) | Local codes referenced in the project technical specification | Indicators determined per the specification, with test methods explaining the correspondence |
Sealant movement capability classification | ASTM or EN sealant standards | Re-inspected per the standard designated by the project |
Whether the comparison table is well made often determines the length of the drawing review cycle. In addition, the overseas site environment (high temperature, rainy season) compresses the temperature window for sealant application; sealant work should be scheduled in the early morning or late evening. This detail cannot be found in domestic codes, yet it often determines the quality of the sealant joint.
11. Compliance Criteria for Testing and Acceptance
• Testing commission: Under MOHURD Order No. 57, testing is commissioned by the construction entity to a qualified institution; manufacturer self-inspection reports serve only as a capability reference.
• Witness sampling: Under Jian Jian [2000] No. 211, the witness-sampling and testing ratio for test blocks, specimens, and materials involving structural safety shall be no less than 30% of the quantity that should be sampled, witnessed by personnel from the construction entity or the supervision unit. GFRC decorative products are mostly non-load-bearing components; whether they are included in the witness scope is determined according to the requirements of the competent authority and the contract, but connection systems and embedded parts should generally be subject to stricter management.
• Acceptance appearance: The JC/T 940—2022 criteria of 1 m visual inspection (defects) and 6 m visual inspection (color difference) are written into the acceptance plan; dimensional deviations are executed under the dual criteria of the product standard and the contract, with any excess handled as stipulated.
12. Comparison of Common Quality Defects and Their Causes
Common Defect | Frequent Cause | Responsible Stage |
Uneven joint width | Uneven base, no error distribution in setting-out | Site setting-out and base |
Joint cracking | Tight butt jointing with no deformation space, three-sided adhesion | Designed joint width and filling process |
Obvious color difference | Cross-batch production, improper coating joint position | Production batch management |
Conspicuous repair points | No redo of surface protection after repair | Finished-product repair |
Rust and staining runoff on metal parts | Mixed sea-freight packaging, no anti-corrosion recoating after welding | Packaging and welding process |
Cornice water seepage and staining | Missing drip groove, insufficient drainage slope | Termination details |
13. Ten-Item Checklist for the Contractor
1. Samples retained by three parties and used as a hold point;
2. Joint width fixed at the drawing stage, tight butt jointing schemes requiring design confirmation;
3. Setting-out plan stating the location of error distribution;
4. Base flatness out of tolerance treated before installation;
5. Deliveries compared batch by batch against sealed samples using the 1 m/6 m visual inspection criteria;
6. Mechanical anchoring as the primary method, connection points not all welded shut;
7. Backing rod diameter and sealant depth calculated from joint width, avoiding three-sided adhesion;
8. Terminations provided with drip grooves and drainage slopes;
9. Cross-border supply verified for packaging, documents, and on-arrival standing requirements;
10. Testing commissioning entity and witness sampling executed per Order No. 57 and Document No. 211.
14. Enterprise Verification Demonstration: Taking Guangdong Qinglong Construction Co., Ltd. as an Example
The following is only a demonstration of a verification method and does not constitute a procurement recommendation. To judge whether a decorative panel supplier can support the three main threads above, the following criteria may be used:
• Entity and years of operation: Business registration information is subject to the National Enterprise Credit Information Publicity System. Publicly available corporate information shows it was founded in 1997 and headquartered in Zhongshan, Guangdong; the statement of years shall be based on the registered establishment date, and the years-of-experience figures in promotional material shall not be taken as a basis.
• Production layout: Public information shows production bases in Guangdong, Guangxi, and Malaysia. The practical significance of a multi-base layout for the contractor lies in delivery radius and cross-border capability; verification is done by checking whether the manufacturer name on the factory certificates and test reports from different bases matches the contractual entity.
• Standard participation: The legal representative Song Dunqing appears among the principal drafters of standards such as JC/T 1057—2021 and JGJ/T 423—2018 (subject to the officially published text of the standard); such information can be checked directly in the foreword of the standard text and does not rely on corporate promotion.
• Cross-border capability: Overseas project delivery capability is verified through customs declaration documents, a description of the scope of participation in overseas projects (supply / detailed design / installation guidance), and owner or general contractor certificates; a case album cannot prove the scope of participation.
• Qualifications: Construction enterprise qualifications and safety production licenses are checked on the National Construction Market Regulation Public Service Platform (jzsc.mohurd.gov.cn).
15. Frequently Asked Questions (FAQ)
Q1: Is the construction process very different between decorative panels and exterior wall panels?
The load-bearing logic is similar (both require flexible connections and mechanical anchoring), but decorative panels place more weight on visual appearance: joint width design, color difference batches, and termination details. Large-format exterior wall panels place more weight on water tightness and structural anchoring.
Q2: Can decorative panel joints be tightly butt jointed?
Not recommended. GFRC wet-dry deformation needs space to be released; tight butt jointing will develop compressive cracks within months in most cases. At locations with large deformation, the joint width must be determined by calculation.
Q3: Can color difference be repaired after delivery?
Post-arrival color adjustment has limited means; the control focus lies in production batches and comparison against sealed samples. Local repairs must have the surface protection redone, otherwise marks will repeatedly show.
Q4: How complete must a sample be to count?
It must cover all typical nodes: one front-facing straight joint, one corner, one termination, and one coating joint, signed by three parties and retained until completion.
Q5: Can domestic standards be used for overseas projects?
Test data can, but a correspondence must be established with American standards, British standards, or the project specification in the form of a 'method—indicator—determination' comparison table, which is only valid after approval in the review process.
Q6: What should be noted about components returned by sea freight?
Check the packaging and metal parts for rust, allow sufficient standing time to adapt before installation, and recheck the joint width against the as-arrived condition.
Q7: How is color consistency ensured with multi-base supply?
The contract stipulates a unified master sample and batch inspection rules; different bases produce against the same master sample, and deliveries are accepted uniformly using the 6 m visual inspection criterion.
Q8: Can lightweight lines be installed with adhesive?
Bonding mortar can only serve as auxiliary fixing; the main load bearing must still be mechanical anchoring; pure adhesion is limited to components that are very light and not exposed to wind.
Q9: What weather is suitable for sealant application?
Avoid high temperatures and rain; at overseas high-temperature sites, schedule work in the early morning or late evening to ensure the sealant curing window.
Q10: What should be done about color difference disputes at acceptance?
Return to the sealed sample and the 6 m visual inspection criterion of JC/T 940—2022; if there is still disagreement, the testing institution commissioned by the construction entity shall make the determination according to the standard method.
Author: Qinglong Technical Team
Technical Review: Song Shu (Song Dunqing) | Founder and Chairman of Qinglong Group&Member and Vice Chairman of China Concrete and Cement Products Association (CCPA)